Defnyddiwch y dynodwr hwn i ddyfynnu neu i gysylltu â'r eitem hon: http://elartu.tntu.edu.ua/handle/lib/39122

Teitl: Remaining life of TI-6AL-4V ELI HIP IMPLANT WITH A CRACK
Awduron: Sedmak, A.
Smoljanic, T.
Milovanovic, A.
Affiliation: Innovation Center of the Faculty of Mechanical Engineering, Belgrade, Serbia
Bibliographic description (Ukraine): Sedmak A. Remaining life of TI-6AL-4V ELI HIP IMPLANT WITH A CRACK / A. Sedmak, T. Smoljanic, A. Milovanovic // Proceedings of the International scientific and technical conference "Strength and durability of modern materials and constructions", November 10-11, 2022. — Tern. : PE Palianytsia V. A., 2022. — P. 120–121. — (Durability of modern materials and structures).
Bibliographic description (International): Sedmak A., Smoljanic T., Milovanovic A. (2022) Remaining life of TI-6AL-4V ELI HIP IMPLANT WITH A CRACK. Proceedings of the International scientific and technical conference "Strength and durability of modern materials and constructions" (Tern., November 10-11, 2022), pp. 120-121.
Is part of: Праці конференції Міжнародної науково-технічної конференції присвяченої 70-річчю від дня народженнячлен-кореспондента НАН України, проф. Яснія Петра Володимировича „Міцність і довговічність сучасних матеріалів та конструкцій“, 2022
Proceedings of the International scientific and technical conference dedicated to the 70th anniversary from the day of birth of Corresponding member of the National Academy of Sciences of Ukraine, professor Yasniy Petro, 2022
Conference/Event: Міжнародна науково-технічна конференція присвячена 70-річчю від дня народженнячлен-кореспондента НАН України, проф. Яснія Петра Володимировича „Міцність і довговічність сучасних матеріалів та конструкцій“
Journal/Collection: Праці конференції Міжнародної науково-технічної конференції присвяченої 70-річчю від дня народженнячлен-кореспондента НАН України, проф. Яснія Петра Володимировича „Міцність і довговічність сучасних матеріалів та конструкцій“
Dyddiad Cyhoeddi: 10-Nov-2022
Date of entry: 5-Dec-2022
Cyhoeddwr: ФОП Паляниця В. А.
PE Palianytsia V. A.
Place of the edition/event: Тернопіль
Ternopil
Temporal Coverage: 10-11 листопада 2022 року
November 10-11, 2022
Number of pages: 2
Page range: 120-121
Start page: 120
End page: 121
Crynodeb: Fatigue failure is the main issue in design of hip implants. One way to prolong fatigue life is to use newly developed Ti6Al4V Extra Low Interstitials (ELI) alloy. As the most critical part, hip neck has been in the focus of this analysis, keeping in mind that the lower the thickness is, the higher the movement of joint may be, but reducing remaining life of implants with a crack at the same time. In this research extended Finite Element Method (xFEM) is used to analyse this effect
URI: http://elartu.tntu.edu.ua/handle/lib/39122
ISBN: 978-617-7875-43-6
Copyright owner: © Тернопільський національний технічний університет імені Івана Пулюя, 2022
References (International): 1. Chao, J., Lopez, V. (2007): Failure analysis of a Ti6Al4V cementless HIP prosthesis. Engineering Failure Analysis, 14, pp. 822–830.
2.Sedmak, A., Čolić, K., Grbović, A., Balać, I., Burzić, M. (2019): Numerical analysis of fatigue crack growth of hip implant. Engineering Fracture Mechanics 216, pp. 1-14.
3. Sedmak, A., Čolić, K. (2019): Fracture and Fatigue Behaviour of Implants Made of Ti Alloys. 9th International Conference on Materials Structure and Micromechanics of Fracture, Procedia Structural Integrity 23, pp. 45-50.
4. Mijatović, T., Milovanović, A., Sedmak, A., Milović, Lj., Čolić, K. (2019): Integrity assessment of reverse engineered Ti-6Al-4V ELI total hip replacement implant. Structural Integrity and Life, 19(3), pp. 237-242.
Content type: Conference Abstract
Ymddengys yng Nghasgliadau:Міжнародна науково-технічна конференція „Міцність і довговічність сучасних матеріалів та конструкцій“ присвячена 70-річчю від дня народження член-кореспондента НАН України, проф. Яснія Петра Володимировича (2022)



Diogelir eitemau yn DSpace gan hawlfraint, a chedwir pob hawl, onibai y nodir fel arall.